AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer AKG Polymers
Trade Name Vision PP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineering, Construction, Horticulture, ElectronicsInformation provided by AKG Polymers BV
Physical Properties Metric English Comments
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
Internal
Filler Content 18 - 22 %
18 - 22 %
Internal
Melt Flow 12 - 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 - 15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
Internal
Flexural Modulus >= 2.00 GPa
>= 290 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched >= 0.200 J/cm²

@Temperature 23.0 °C
>= 0.952 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
Descriptive Properties Value Comments
Application Area automotive
Color Black
Filler Type Talc
Non-virgin Polymer Content (%), Min 75
Process injection moulding