AIM 88Au/12Ge Solder for Photonic Packaging

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer AIM Specialty Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AIM 88Au/12Ge Solder for Photonic Packaging.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Physical Properties Metric English Comments
Density 14.7 g/cc
0.531 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1280 MPa
185000 psi
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 °C
7.22 µin/in-°F

@Temperature 68.0 °F
Melting Point 356 °C
673 °F
Solidus 356 °C
673 °F
Liquidus 356 °C
673 °F
Component Elements Properties Metric English Comments
Germanium, Ge 12 %
12 %
Gold, Au 88 %
88 %
Descriptive Properties Value Comments
Creep Resistance Excellent