AIM 80Au/20Sn Solder for Photonic Packaging

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer AIM Specialty Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AIM 80Au/20Sn Solder for Photonic Packaging.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Physical Properties Metric English Comments
Density 14.5 g/cc
0.524 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1900 MPa
276000 psi
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 20.0 °C
8.89 µin/in-°F

@Temperature 68.0 °F
Melting Point 280 °C
536 °F
Solidus 280 °C
536 °F
Liquidus 280 °C
536 °F
Component Elements Properties Metric English Comments
Gold, Au 80 %
80 %
Tin, Sn 20 %
20 %
Descriptive Properties Value Comments
Creep Resistance Excellent