A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer A.D. Compound
Trade Name Adene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A.D. Compound
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Filler Content 40 %
40 %
ISO 3451 / 1
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ISO 868
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527
Elongation at Break 50 %
50 %
ISO 527
Elongation at Yield 8.0 %
8.0 %
ISO 527
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75
Vicat Softening Point 76.0 °C
169 °F
49 N; ISO 306