Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QSil 430 QSI Quantum Silicones Silicone Potting Material  (discontinued **)

Category Polymer , Thermoset , Silicone
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QSil 430 QSI Quantum Silicones Silicone Potting Material  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, quick curing, flame retardant, great adhesion to a variety of substrates.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
"B" component
1.41 g/cc
1.41 g/cc
"A" component
Viscosity 20000 cP
20000 cP
"B" component
20000 cP
20000 cP
"A" component
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
catalyzed
Tensile Strength, Yield >= 2.80 MPa
>= 406 psi
catalyzed
Elongation at Break >= 100 %
>= 100 %
catalyzed
Tear Strength >= 2.63 kN/m
>= 15.0 pli
catalyzed
Thermal Properties Metric English Comments
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 3.0

@Frequency 1000 Hz
3.0

@Frequency 1000 Hz
Dielectric Strength 18.9 kV/mm
480 kV/in
Processing Properties Metric English Comments
Pot Life 6.0 - 10 min
6.0 - 10 min
anti-slump
Descriptive Properties Value Comments
Color Beige
"B" component
Black
"A" component