Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QLE 1050 QSI Quantum Silicones 30 Durometer Clear, Addition Cure, 1-part Elastomer for Coating

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QLE 1050 QSI Quantum Silicones 30 Durometer Clear, Addition Cure, 1-part Elastomer for Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QLE 1050 is a 100% silicone solids elastomer designed for use as a conformal coating, but can also be used for cloth coating applications. Key Features: 100% solids Transparent, ideal for pigmentation Fast cure at elevated temperaturesPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Viscosity 500 cP
500 cP
Storage Temperature <= 4.44 °C
<= 40.0 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
cured 10 mins @ 150°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
cured 10 mins @ 150°C
Maximum Service Temperature, Air 204 °C
399 °F
cured 10 mins @ 150°C
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
cured 10 mins @ 150°C
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
cured 10 mins @ 150°C
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 200 °C
0.250 hour

@Temperature 392 °F
<= 60.0 min

@Temperature 150 °C
<= 1.00 hour

@Temperature 302 °F
Descriptive Properties Value Comments
Color Clear/Light Brown