A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of PP 3369-01 are packaging articles such as caps and closures and large containers. PP 3369-01 meets FDA Regulation 21 CFR 177.1250, for all food packaging applications at temperatures not exceeding 212°F (100°C).Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.907 g/cc
0.907 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648