Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 4.572 GPa
663.1 ksi
ASTM D790
Izod Impact, Notched 1.75 J/cm
3.28 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved