Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ISO 1183/1
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min; ISO 527
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
ISO 75