Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 8.0 - 16 g/10 min
8.0 - 16 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D638
Flexural Modulus 3.87 GPa
561 ksi
ASTM D790
Izod Impact, Notched 0.570 J/cm
1.07 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ASTM D648
Users viewing this material also viewed the following: