Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 0.870 GPa
126 ksi
ASTM D790
Izod Impact, Notched 5.00 J/cm
9.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648