A. Schulman POLYBLAK™ 4676 Black Color Concentrate, 50% Carbon Black Based In LLDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBLAK™ 4676 Black Color Concentrate, 50% Carbon Black Based In LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBLAK® Black 4676 is a black color concentrate containing 50% carbon black based in LLDPE. This masterbatch is designed to provide uniform opacity and a regular blue undertone with pigment particle size of 65 nanometers. POLYBLAK® 4676 is formulated for use in polyolefin film, drip tape/tube and injection molding applications. POLYBLAK® 4676 is typically recommended for use at addition levels between 1 and 5%.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Carbon Black Loading 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789