A. Schulman POLYBLAK™ 4651SF Universal Black Color Concentrate, 50% Carbon Black in EVA

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBLAK™ 4651SF Universal Black Color Concentrate, 50% Carbon Black in EVA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBLAK® Black 4651SF is a universal black color concentrate containing 50% carbon based in EVA. This product is also produced without the use of stearates or any other lubricants. This masterbatch is designed to provide good opacity and a regular blue undertone with pigment particle size of 70 nanometers. POLYBLAK® Black 4651SF is formulated for use in injection molding and extrusion applications and is typically recommended for use at 5% addition levels.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Carbon Black Loading 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789