A. Schulman POLYBATCH™ White 8350 AP Concentrate Based In LDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ White 8350 AP Concentrate Based In LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® 8350 AP is an advanced performance white color concentrate containing 50% TiO2 based in LDPE. This product has been specifically engineered to provide improved resistance to phenolic yellowing/pinking, while optimizing whiteness and thermal stability. POLYBATCH® 8350 AP has been designed to provide optimal dispersion and excellent letdown mixing in LDPE, LLDPE, and HDPE film and sheet applications. POLYBATCH® 8350 AP can also be used in injection and blow molding applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 32
pellets/gram
Users viewing this material also viewed the following: