A. Schulman POLYBATCH™ Poly White P80494PF Concentrate Based In Polypropylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Poly White P80494PF Concentrate Based In Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® P80494PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color polypropylene film, extrusion, and molding applications. This product has been specially engineered to provide improved resistance to phenolic yellowing/pinking. POLYBATCH® P80494PF is heavy metal free and is typically recommended for use at 30% addition levels.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 55
pellets/gram