Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm

@Thickness 3.20 mm
0.0060 - 0.010 in/in

@Thickness 0.126 in
72 hr; ISO 294
0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
15 sec delay; ISO 868
Tensile Strength, Ultimate 23.0 MPa
3340 psi
at max load; ISO 527
Elongation at Break 375 %
375 %
ISO 527
Flexural Modulus 0.988 GPa
143 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C

@Thickness 3.20 mm
144 °F

@Thickness 0.126 in
ISO 75