Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 110 MPa
16000 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 11.2 GPa
1620 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.38 J/cm
8.21 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 258 - 268 °C
496 - 514 °F
Deflection Temperature at 0.46 MPa (66 psi) 243 °C
469 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved