A. Schulman ComAlloy Hiloy® 132 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 132 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Ultimate 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 4.70 GPa
682 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
291 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 225 °C
437 °F
Approximate middle barrel temperature.