A. Schulman ComAlloy E-16901B PPS Alloy, Electrically Conductive - Carbon Fiber Filled

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Conductive
Manufacturer A. Schulman ComAlloy
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy E-16901B PPS Alloy, Electrically Conductive - Carbon Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 24.0 GPa
3480 ksi
ASTM D790
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 280 - 290 °C
536 - 554 °F
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 10.0 ohm-cm
1.00 - 10.0 ohm-cm
Surface Resistance 10 - 100 ohm
10 - 100 ohm
Copyright © lookpolymers.com All Rights Reserved