Material Notes:
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Ultimate 33.0 MPa
4790 psi
ASTM D638
Elongation at Break 41 %
41 %
ASTM D638
Flexural Strength 52.0 MPa
7540 psi
ASTM D790
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 195 - 215 °C
383 - 419 °F
Deflection Temperature at 0.46 MPa (66 psi) 151 °C
304 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
ASTM D648