Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with Carbon Black Filler
Manufacturer A. Schulman ComAlloy
Trade Name Comshield®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 48.0 MPa
6960 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Unnotched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 100 ohm-cm
10.0 - 100 ohm-cm
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm