Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman ComAlloy
Trade Name Aqualoy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability and high strength traits into a unique property blend.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Ultimate 81.0 MPa
11700 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 108 MPa
15700 psi
ASTM D790
Flexural Modulus 5.70 GPa
827 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 161 °C
322 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 246 °C
444 - 475 °F