Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M XLD3000 Glass Bubbles

Category Ceramic , Glass
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M XLD3000 Glass Bubbles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with a variety of polymers to reduce the overall thermal conductivity of the composite. These composites can be coated or incorporated into deep sea oil pipelines to improve the flow assurance properties of the system. The high strength of XLD3000 glass bubbles can withstand both the high processing pressure of polymer extrusion and the pressure of seawater in many applications. The XLD3000 glass bubbles have isostatic crush strengths of 3,000 psi with a minimum of 90% survival.Information provided by 3M
Physical Properties Metric English Comments
Density 0.230 g/cc
0.00831 lb/in³
Volatiles 0.40 %
0.40 %
Particle Size 30 µm
30 µm
diameter
pH 9.5
9.5
5% loading in water
Thermal Properties Metric English Comments
Thermal Conductivity 0.780 W/m-K

@Temperature 50.0 °C
5.41 BTU-in/hr-ft²-°F

@Temperature 122 °F
Softening Point 600 °C
1110 °F
Descriptive Properties Value Comments
Alkalinity 0.4 milliequivalents/gram
Appearance White, powdery
unaided eye
Shape Hollow spheres with thin walls
Users viewing this material also viewed the following: