Material Notes:
A high tack and fast drying mist spray adhesiveFeatures:Securely bonds many lightweight materials such as attaching foils, carpeting, lightweight paper, cardboard, felt, and cloth to painted or unpainted metals, wood.Meets CARB/OTC VOC RequirementsHelps contribute to LEED® credits.GREENGUARD Indoor Air Quality Certified®Information provided by 3M
Physical Properties Metric English Comments
Density 0.791 g/cc
0.0286 lb/in³
Solids Content 19.4 %
19.4 %
Descriptive Properties Value Comments
Appearance Translucent
Base Synthetic elastomer