3M Scotchkote™ GP 830 WB Epoxy Primer

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ GP 830 WB Epoxy Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchkote WB Epoxy Primer GP 830 is a member of a range of Scotchkote waterborne coatings and has been specifically developed as a primer/tie coat for use on sealed mineral surfaces and existing coating.Information provided by 3M
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Solids Content 46 %
46 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Thickness 40.6 microns
1.60 mil
Dry
88.9 microns
3.50 mil
Wet
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Dry
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
Touch Dry
480 min
8.00 hour
Hard Dry
10100 min
168 hour
Full Cure
Shelf Life 24.0 Month

@Temperature 5.00 - 32.0 °C
24.0 Month

@Temperature 41.0 - 89.6 °F
Descriptive Properties Value Comments
Appearance Off white