Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchkote™ FG 514 Urethane Ceramic Lining

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ FG 514 Urethane Ceramic Lining.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Urethane Ceramic Lining FG 514 has been specifically developed as a 100% solids polyceramic coating with a degree of flexibility for lining and resurfacing equipment operating in fluid flow environments.Product Features:Combines good application characteristics with good cavitations and erosion resistanceDesigned for application by stiff brush or squeegeeProvides outstanding protection against impingementPrimarily designed for use on propellers, kort nozzles, guide vanes, and turbines. Information provided by 3M
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Solids Content 100 %
100 %
Thickness 1000 microns
39.4 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.5 MPa
2830 psi
Abrasion 0.080
0.080
[g] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Processing Properties Metric English Comments
Cure Time 120 min
2.00 hour
Touch Dry
240 min
4.00 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Gray
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved