Material Notes:
Scotchkote Urethane Primer FB 856 has been specifically developed as a primer/sealer for porous mineral, timber and asphalt surfaces used on floors and roofs.Product Features:Combines good application characteristics with fast drying capabilitiesDesigned for use prior to application of Scotchkote urethane finishesSuitable for brush and roller application.Information provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Solids Content 65 %
65 %
Volatile Organic Compounds (VOC) Content 312 g/l
312 g/l
Thickness 76.2 microns
3.00 mil
dry
114 microns
4.50 mil
wet
Processing Properties Metric English Comments
Cure Time 120 min
2.00 hour
Touch Dry
Descriptive Properties Value Comments
Appearance Clear
Users viewing this material also viewed the following: