Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchkote™ 165HB Urethane Coating

Category Polymer , Thermoset
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 165HB Urethane Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchkote Urethane Coating 165HB is a two component 100% solids urethane coating used for the internal and external protection of steel and concrete pipes, tanks, and vessels. It can be used in many different immersion conditions, including sea, foul and raw water; also in chemically polluted, marine or underground environments. Scotchkote urethane coating 165HB is specifically designed for plural feed hot airless spray application. As such it permits single coat applications of between 0.5 mm and 2 mm dft.Information provided by 3M
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Water Absorption 0.26 %
0.26 %
24 hrs; ASTM D570
1.19 %
1.19 %
21 days; ASTM D570
Thickness 1020 microns
40.0 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ASTM D2240
Tensile Strength at Break 14.3 MPa
2070 psi
ASTM D638
Elongation at Break 24 %
24 %
ASTM D638
Impact Test 7.00 J
5.16 ft-lb
1/4" steel plate; ASTM G14 (modified)
Abrasion 98
98
[mg] loss per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Minimum Service Temperature, Air 0.000 °C
32.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 180 min
3.00 hour
Touch Dry
360 min
6.00 hour
Hard Dry
10100 min
168 hour
Full Cure
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Gray