3M Scotchkote™ 152LV Epoxy Coating

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 152LV Epoxy Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Coating 152LV has been specifically developed as a surface tolerant anti corrosive coating for steel structures.Product Features:Combines good application characteristics with excellent corrosion protection and chemical resistance.Is designed for application by brush at thicknesses of up to 1mm in a single application.Is suitable for use on grit blasted steel, mechanically prepared steelwork or high pressure water cleaned steel.Adhesion: Excellent to both blast cleaned and mechanically prepared surfaces.Corrosion: Resistance Excellent even under immersion conditions.Chemical Resistance: Unaffected by short term contact with most industrial chemicals.Temperature Resistance: Suitable for use up to 100°C dry heat Information provided by 3M
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Solids Content 99.2 %
99.2 %
Volatile Organic Compounds (VOC) Content 14 g/l
14 g/l
mixed
Thickness 254 - 1020 microns
10.0 - 40.0 mil
Processing Properties Metric English Comments
Cure Time 720 min
12.0 hour
Touch Dry
960 min
16.0 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Beige, gray or black