3M Scotchcal™ 3650-12 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcal™ 3650-12 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 19.0 MPa
>= 2760 psi
Peel Strength 0.701 kN/m
4.00 pli
Adhesion to Fruehauf pre-painted panels
0.877 kN/m
5.00 pli
Adhesion to ABS
0.877 kN/m
5.00 pli
Adhesion to Acrylic enamel
0.877 kN/m
5.00 pli
Adhesion to Chrome
1.05 kN/m
6.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Descriptive Properties Value Comments
Appearance Black
Users viewing this material also viewed the following: