3M ScotchPad™ 822 Label Protection Tape Pad

Category Polymer , Adhesive
Manufacturer 3M
Trade Name ScotchPad™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M ScotchPad™ 822 Label Protection Tape Pad.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ ScotchPad™ Label Protection Tape Pad 822 is a pre-cut pad formed with layered high-performance tape sheets featuring durable 3M™ ScotchPad™ polypropylene film backing that is strong, conformable, and resistant to impact shock, Tape sheets are coated with an aggressive adhesive to provide excellent adhesion to many types of surfaces. Each piece of tape is coupled with a liner material for easy handling and dispensing, without the need for a dispenser. Tape sheets are used for repairing broken packages, for label protection, industrial covering applications, and protection of surfaces in manufacturing processes. Tuck-in flap boxes are securely closed with these tape sheets.Information provided by 3M
Physical Properties Metric English Comments
Thickness 78.7 microns
3.10 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.76 MPa
1130 psi
Longitudinal; ASTM D3759
15.5 MPa
2250 psi
Transverse; ASTM D3759
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.60259 kN/m
3.4375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive hot melt rubber resin
Appearance Transparent