Material Notes:
3M™ ScotchPad™ Custom Printed Marking Taps 818CP are individual paper tags laminated to the strongest conformable backing and most consistent pressure-sensitive hot-melt adhesive system available. These tags have adhesive below one short edge for strong attachment to many surfaces. The protective, strong 3M™ Scotchpro™ Polypropylene top surface allows clear reading of the printed material but shields the print from abrasion, dirt, liquids. These tags are stacked 25 to a pad with a backsheet. The tags can be placed on flat surfaces or wrapped around thinner objects. When the adhesive is placed against the tag’s back paper surface, the paper will tear upon removal and provide tamper evidence.Information provided by 3M
Physical Properties Metric English Comments
Thickness 78.7 microns
3.10 mil
Tape; ASTM D3652
81.3 microns
3.20 mil
Paper; ASTM D3652
155 microns
6.10 mil
Tab; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.57 MPa
1100 psi
Longitudinal; ASTM D3759
15.1 MPa
2200 psi
Transverse; ASTM D3759
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.60259 kN/m
3.4375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Blue, red, white yellow, or custom