Material Notes:
3M™ ScotchPad™ Tape Pad 3750P is a pre-cut pad formed with layered, high-performance tape sheets featuring durable 3M™Scotchpro™ film backing that is strong, conformable, and resistant to impact shock. Tape sheets are coated with an aggressive adhesive to provide excellent holding power to many surfaces. Each piece of tape is coupled with a strip of liner material for easy handling and application, without the need for a dispenser.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3652
78.7 microns
3.10 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.76 MPa
1130 psi
Longitudinal; ASTM D3759
15.5 MPa
2250 psi
Transverse; ASTM D3759
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.60259 kN/m
3.4375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure-sensitive synthetic rubber resin
Appearance Transparent, tan