Material Notes:
3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small diameter applications. These film materials utilize 3M™ Adhesive 320 which offers high initial tack and excellent adhesion to a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics such as polyethylene.Information provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Adhesive
50.8 microns
2.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.64642 kN/m
3.6875 pli
Polypropylene, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
0.877 kN/m
5.00 pli
ABS Plastic, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
0.877 kN/m
5.00 pli
Acrylic Paint, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
0.877 kN/m
5.00 pli
Chrome, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
1.0408 kN/m
5.9375 pli
Aluminum, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
1.118 kN/m
6.375 pli
Stainless Steel, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 °C
203 °F
Permanent
150 °C
302 °F
Short term
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Short term
-60.0 °C
-76.0 °F
Permanent
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 320 High Tenacity Acrylic
Liner Yellow Glassine Liner