Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch-Weld™ LO100 Low Odor Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ LO100 Low Odor Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low odor but also low blooming. The residues (chlorosis) of the joint area are eliminated to improve appearance in cosmetically critical applications. Lower odor can improve worker comfort in work areas where ventilation is limited. These products reduce the requirement for sophisticated ventilation systems that may be necessary when dispensing other cyanoacrylates. LO100 is a low viscosity cyanoacrylate for general purpose low odor bonding.Information provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Viscosity 100 cP
100 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.5 MPa
2100 psi
cured; ISO 6922
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.0 °C
160 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.167 - 1.00 min
0.00278 - 0.0167 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid
Users viewing this material also viewed the following: