3M Scotch-Weld™ HT700 High Temperature Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ HT700 High Temperature Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a medium viscosity high temperature resistant toughened cyanoacrylate that has some gap-filling capabilities.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 700 cP
700 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 106 °C
223 °F
Continuous
121 °C
250 °F
Intermittent
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Continuous
-54.0 °C
-65.2 °F
Intermittent
Processing Properties Metric English Comments
Cure Time 0.250 - 0.667 min
0.00417 - 0.0111 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid
Users viewing this material also viewed the following: