3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity version of CA40 and better void filling capabilities.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 400 - 600 cP
400 - 600 cP
Mechanical Properties Metric English Comments
Shear Strength 0.241 MPa
35.0 psi
Overlap, Nitrile Rubber; ASTM D1002-64
0.379 MPa
55.0 psi
Overlap, Neoprene Rubber; ASTM D1002-64
6.21 MPa
900 psi
Overlap, ABS; ASTM D1002-64
6.89 MPa
1000 psi
Overlap, Rigid PVC; ASTM D1002-64
10.3 MPa
1500 psi
Overlap, Steel; ASTM D1002-64
10.3 MPa
1500 psi
Overlap, Aluminum; ASTM D1002-64
Peel Strength 0.175 - 0.351 kN/m
1.00 - 2.00 pli
T-Peel
Processing Properties Metric English Comments
Cure Time 0.083333 - 0.666666 min
0.0013889 - 0.0111111 hour
Descriptive Properties Value Comments
Appearance Clear