3M Scotch-Weld™ AC77 Instant Adhesive Primer

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ AC77 Instant Adhesive Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Instant Adhesive Primer AC77 is designed for difficult-to-bond, low surface energy plastics such as polypropylene, polyethylene, and PTFE. This primer needs to be applied to each low surface energy substrate surface.Information provided by 3M
Physical Properties Metric English Comments
Density 0.800 g/cc
0.0289 lb/in³
Viscosity >= 3.0 cP
>= 3.0 cP
Descriptive Properties Value Comments
Appearance Colorless Liquid