Material Notes:
Features: It is a sprayable, synthetic elastomer based adhesive for bonding many lightweight materials such as felt, cork, cardboard, and paper to metal and other substratesIdeal for palletizing “all-plastic” shipping bags, Holds bags in place during storage and shipment. When unstacking, bags separate easily with no bag tear.Fast tacking; ideal for low pressure spray with minimal misting and cobwebbing. Offers high coverage and long bonding rage.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 36 - 38 %
36 - 38 %
Brookfield Viscosity 100 - 4000 cP
100 - 4000 cP
RVF #4 sp @ 20 rpm @ 27°C
Mechanical Properties Metric English Comments
Peel Strength 2.10 kN/m
12.0 pli
180°, Scott Tensile Tester
Thermal Properties Metric English Comments
Flash Point -29.0 °C
-20.2 °F
TCC
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance Translucent
Base SBR