3M Scotch-Weld™ 3794 Hi Tack PSA Bulk only Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 3794 Hi Tack PSA Bulk only Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sprayable high tack PSA for bonding plastic, paper, metals, die-cut labelsInformation provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 15000 cP

@Temperature 163 °C
15000 cP

@Temperature 325 °F
Mechanical Properties Metric English Comments
Peel Strength 2.80 kN/m
16.0 pli
on canvas
Thermal Properties Metric English Comments
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28-99