3M Scotch-Weld™ 1469 One-Part Epoxy Adhesives and Metal Primer

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 1469 One-Part Epoxy Adhesives and Metal Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Temperature strength and Low ViscosityInformation provided by 3M
Physical Properties Metric English Comments
Viscosity 60000 cP
60000 cP
Mechanical Properties Metric English Comments
Shear Strength 21.7 MPa

@Temperature -55.0 °C
3150 psi

@Temperature -67.0 °F
Overlap
24.8 MPa

@Temperature 121 °C
3600 psi

@Temperature 250 °F
Overlap
25.5 MPa

@Temperature 24.0 °C
3700 psi

@Temperature 75.2 °F
Overlap
25.5 MPa

@Temperature 82.0 °C
3700 psi

@Temperature 180 °F
Overlap
Peel Strength 0.351 kN/m
2.00 pli
T-Peel
Processing Properties Metric English Comments
Cure Time 120 min

@Pressure 0.0689 MPa,
Temperature 177 °C
2.00 hour

@Pressure 10.0 psi,
Temperature 351 °F