Material Notes:
Scotch® Super 33+™ Vinyl Electrical Tape is a premium grade, 7 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is conformable for cold weather application down to -18°C. It has excellent resistance to abrasion, moisture, alkalies, acids, corrosion and varying weather conditions (including ultraviolet exposure). The combination of elastic backing and aggressive adhesive provides moisture-tight electrical and mechanical protection with minimum bulk. Scotch® Super 33+™ Vinyl Electrical Tape is UL Listed and is a Canadian Standards Association (CSA) Certified “Insulating Tape”.Information provided by 3M
Physical Properties Metric English Comments
Thickness 178 microns
7.00 mil
Mechanical Properties Metric English Comments
Elongation at Break 100 %

@Temperature -18.0 °C
100 %

@Temperature -0.400 °F
ASTM D1000
250 %

@Temperature 22.0 °C
250 %

@Temperature 71.6 °F
ASTM D1000
Peel Strength 0.307 kN/m

@Temperature 2.00 °C
1.75 pli

@Temperature 35.6 °F
Adhesion to Steel; ASTM D1000
0.307 kN/m

@Temperature 22.0 °C
1.75 pli

@Temperature 71.6 °F
Adhesion to Backing; ASTM D1000
0.657 kN/m

@Temperature -18.0 °C
3.75 pli

@Temperature -0.400 °F
Adhesion to Steel; ASTM D1000
0.657 kN/m

@Temperature -18.0 °C
3.75 pli

@Temperature -0.400 °F
Adhesion to Backing; ASTM D1000
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
ASTM D1000
Dielectric Strength 45.3 kV/mm
1150 kV/in
ASTM D1000
Descriptive Properties Value Comments
Appearance Black