3M Scotch® 899 Filament Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 899 Filament Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Filament Tape 899 is a high performance packaging tape reinforced with continuous glass-yarn filaments that give the tape very high tensile strength and low stretch. The red 3M™ Scotchpro™ Film backing provides excellent abrasion and moisture resistance. The aggressive packaging-grade adhesive is specifically formulated to provide an excellent balance of initial adhesion and long-term holding power to most fiberboard surfaces, including recycled and printed fiberboard surfaces. When used in bundling, reinforcing, or coil tabbing applications, where high temperatures and/or oily surfaces are involved, tests should be conducted per the individual application before extensive use to determine the tape’s suitability.Information provided by 3M
Physical Properties Metric English Comments
Thickness 168 microns
6.60 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.5 MPa
5440 psi
ASTM D3759
Elongation at Break 3.0 %
3.0 %
ASTM D3759
Peel Strength 0.7669 kN/m
4.375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Red