3M Scotch® 8631 Bag Conveying Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 8631 Bag Conveying Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Bag Conveying Tape 8631 is a high-performance tape reinforced with continuous polypropylene mono filaments. Scotch® Tape 8631 is designed to hold polyethylene bags together during shipping loading. The pressure sensitive adhesive is specifically formulated to provide consistent adhesion to polyethylene.Information provided by 3M
Mechanical Properties Metric English Comments
Elongation at Break 30 %
30 %
ASTM D3759
Peel Strength 0.73407 kN/m
4.1875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Clear