3M Scotch® 8347 Carry Handle Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 8347 Carry Handle Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Carry Handle Tape 8347 is a high-performance tape featuring a durable 3M™ Scotchpro™ Film backing that is longitudinal direction and an aggressive rubber resin adhesive especially suited for high shear performance carrying handles that allows for items up to 20 lbs. to be carried easily.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; AFERA 4006
73.7 microns
2.90 mil
Total; AFERA 4006
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.55 MPa
950 psi
AFERA 4004
Elongation at Break 40 %
40 %
AFERA 4005
Peel Strength 0.2410 kN/m
1.375 pli
Adhesion to Polyethylene
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Transparent