3M Scotch® 821 LabelGard™ Film Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 821 LabelGard™ Film Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® LabelGard™ Film Tape 821 is a lightly tented pink film designed for protecting labels and packaging lists. The synthetic adhesive is designed for easy handling and dispensing with low static. It also offers abrasion and moisture protection. Writing on the backing with No. 2 pencils, ball point, and many marking pens makes this label covering tape acceptable by the US Postal Service and UPS.Information provided by 3M
Physical Properties Metric English Comments
Thickness 40.6 microns
1.60 mil
Backing; ASTM D3652
63.5 microns
2.50 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.33 MPa
483 psi
ASTM D3759
Elongation at Break 15 %
15 %
longitudinal; ASTM D3759
Peel Strength 0.27391 kN/m
1.5625 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Transparent pink