Material Notes:
Scotch® Polyethylene Coated Cloth Tape 390 has a durable backing with a rubber adhesive used for applications requiring high strength and moisture resistance.Information provided by 3M
Physical Properties Metric English Comments
Thickness 7.62 microns
0.300 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4070 psi
ASTM D3759
Elongation at Break 12 %
12 %
ASTM D3759
Peel Strength 1.249 kN/m
7.125 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Oliver Green, Silver