Material Notes:
Scotch® Box Sealing Tape 371 is an industrial packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consistent pressure sensitive hot melt synthetic rubber adhesive system.Information provided by 3M
Physical Properties Metric English Comments
Thickness 48.3 microns
1.90 mil
ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.49303 kN/m
2.8125 pli
Adhesion to Steel; ASTM D3330
Film Tensile Strength at Break, MD 8.02 MPa
1160 psi
ASTM D3759
Film Tensile Strength at Break, TD 16.1 MPa
2330 psi
ASTM D3759
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive hot melt rubber-resin
Appearance Blue, clear, green, orange, red, tan, yellow and white