3M Scotch® 2460 Ultimate Paint Edge Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 2460 Ultimate Paint Edge Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Ultimate Paint Edge Masking Tape 2460 uses a thing, yet strong, smooth flat back paper that when used for paint masking gives a sharp paint line with low paint ridge. This backing simplifies the task of making long straight lines but still incorporates the easy of being torn by hand. The acrylic adhesive holds on contact to many surfaces, yet peels away smoothly and cleanly.Information provided by 3M
Physical Properties Metric English Comments
Thickness 2.03 microns
0.0800 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.375 MPa
5710.9 psi
ASTM D3759
Elongation at Break 6.0 %
6.0 %
ASTM D3759
Peel Strength 0.0877 kN/m
0.500 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
for up to 30 min, removes cleanly
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Yellow
Users viewing this material also viewed the following: