3M Scotch™ 2200 Vinyl Mastic Pads and Rolls

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer 3M
Trade Name Scotch™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch™ 2200 Vinyl Mastic Pads and Rolls.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are designed to insulate, moisture seal and pad all connections up to 600 volts, and have excellent resistance to abrasion, moisture, alkalies, acid, copper corrosion and varying weather conditions (including sunlight).Information provided by 3M
Physical Properties Metric English Comments
Water Absorption 0.75 %
0.75 %
ASTM D570
Water Vapor Transmission 3.88 g/m²/day
0.250 g/100 in²/day
ASTM D3833
Thickness 178 microns
7.00 mil
Backing; ASTM D1000
2110 microns
83.0 mil
Mastic-Roll; ASTM D1000
2290 microns
90.0 mil
Composite-Roll; ASTM D1000
3000 microns
118 mil
Mastic-Pad; ASTM D1000
3180 microns
125 mil
Composite-Pad; ASTM D1000
Mechanical Properties Metric English Comments
Elongation at Break 200 %
200 %
ASTM D1000
Peel Strength 2.19 kN/m
12.5 pli
Adhesion to Steel; ASTM D1000
2.19 kN/m
12.5 pli
Adhesion to Polyethylene; ASTM D1000
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
ASTM D1000
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D1000
Descriptive Properties Value Comments
Appearance Black